Focus Pro

Development Trends in Direct RGB Patterning for OLEDoS I

Nov. 2026 | Dr. Noh Chang-ho (Senior Analyst), UBI Research

This Focus Pro reviews development trends in Direct RGB patterning, which forms R, G, and B emitting layers for each subpixel of an OLEDoS without color filters, along three routes: mask evaporation, photolithography, and direct patterning of the emitting material. The main sources are the reverse-taper FSM (Fine Silicon Mask) patent (CN 122959660 A) that Samsung Display published in China on October 23, 2026, and the RGB evaporation system for 12-inch Si wafers that Canon Tokki presented at the 43rd Organic EL Symposium in November. Photolithography-related patents from SEL and Ruixian, the native RGB presentation by INT-Tech and Guanyu at SID 2026, and a Nature paper from ETH Zurich are also covered.

1. Overview: Why OLEDoS Needs Direct RGB

OLEDoS is a small panel in the 0.4–2-inch class used in VR and MR headsets and camera electronic viewfinders (EVFs); because it sits close to the eye, it requires a resolution of 3,000 ppi or more. At this resolution it is difficult to form RGB separately by mask evaporation, so the W-OLED+CF structure, with color filters on a white OLED, has become the mass-production standard. BOE (京东方)’s 0.49-inch 4,496 ppi product and Samsung Display’s OLEDoS for Galaxy XR both use this structure. Because color filters absorb light outside their own wavelength band, emission efficiency is low, and securing luminance is difficult in AR glasses, where losses in waveguide optics are large. Panels for AI and AR glasses are shrinking to the 0.1-inch class; a 0.13-inch VGA (640×480) panel has a pixel pitch of 4 µm, exceeding 6,000 ppi. This size range is currently supplied mainly by micro-LED (JBD) and LCoS (RAONTECH). For OLEDoS, Fraunhofer FEP presented a 0.18-inch prototype with a 2.5 µm pixel pitch in 2023, and Samsung Display unveiled a 0.62-inch RGB OLEDoS prototype for glasses at AWE 2026.

The difficulty of Direct RGB lies in subpixel size. For an RGB stripe layout, the subpixel width shrinks to 2.8 µm at 3,000 ppi and 1.7 µm at 5,000 ppi (Table 1). According to Canon Tokki’s presentation, the alignment precision of evaporation systems for OLED mass production is about ±3 µm on G6H glass substrates, and W-OLED evaporation systems for micro OLED are at the ±10–100 µm level. Separate RGB evaporation requires precision one to two orders of magnitude higher.

Table 1. Pixel density vs. RGB subpixel width

Pixel density (ppi)Pixel pitch (µm)RGB subpixel width (µm)Reference
3,0008.52.8Required level for AR/VR OLEDoS
3,5007.32.4Samsung Display/eMagin FSM demo (SID 2024)
5,0005.11.7Samsung Display RGB OLEDoS (CES 2026)

2. Samsung Display’s Reverse-Taper FSM Patent (CN 122959660 A)

Samsung Display is targeting mass production of RGB OLEDoS in 2028, with equipment orders scheduled for the second half of 2026 and installation in 2027. It unveiled a 5,000 ppi RGB OLEDoS at CES 2026 and an RGB panel of about 40,000 nits at AWE 2026. CN 122959660 A, published on October 23, 2026 (Chinese application 202610486806.9; Korean priority 10-2025-0052543, April 22, 2025), covers the fine pattern layer of the FSM used for this evaporation.

The deposition source (DPS) is located below the mask, and the deposition material passes in turn through the substrate support-layer opening (OP1), the protection-layer opening (OP2), and the fine pattern opening (POP) (Figure 1). The fine pattern layer (PL) is made of single-crystal Si or poly-Si, the protection layer (PRL) and the optional lower layer (LL) of SiOx, and the base layer (BL) of Si. Both the support-layer openings and the fine-pattern openings are designed to widen toward the deposition source.

Figure 1. FSM cross-section and deposition source position

The LPCVD low-stress nitride (LSN) used in conventional FSM pattern layers has high etch resistance and bonding energy, making a reverse-taper profile difficult to form. Samsung Display changed the pattern layer to Si and controlled the cross-sectional profile with SF₆ plasma etching. Because the pattern grid (PGD) is wider on the substrate side than on the deposition-source side, the openings (POP) are wide on the source side and narrow on the substrate side (Figure 2). This structure reduces the extent to which obliquely incident deposition particles are blocked by the sidewalls. The taper angle (A1) is about 80° or more and less than 90°, with 80–85° given as an example for minimizing shadow.

Figure 2. Reverse-taper pattern: schematic (left) and fabricated cross-section (right)

Fabrication proceeds by stacking a first SiOx protection layer, a Si or poly-Si intermediate layer, and a second SiNx protection layer on a Si wafer, then forming the reverse-taper pattern on the front side by Bosch dry etching and machining the support-layer openings on the back side (Figure 3, Table 2). In the embodiments, the SiNx hard mask used for etching is 400–500 Å (40–50 nm) thick.

Figure 3. FSM fabrication: (a) front pattern etch, (b) back opening, (c) after protection-layer removal

Table 2. FSM fabrication sequence

StepProcess
S100–S200Prepare Si wafer; stack SiOx / Si (or poly-Si) / SiNx
S300Lithography, then Bosch dry etch to form reverse-taper pattern
S400–S500Remove back-side SiNx and Si layer; etch Si substrate to form support openings (wet etch possible)
S600Remove remaining front-side SiNx hard mask

Source: CN 122959660 A

During the same period, Samsung Display also published US applications that prevent sagging of the mask membrane using piezoelectric tension (US 2026/0275488 A1) and a magnetic layer (US 2026/0062789 A1).

3. Evaporation Equipment: Canon Tokki and Sunic System

At the 43rd Organic EL Symposium, held in Fukuoka, Japan, on November 12–13, Canon Tokki presented a prototype RGB evaporation system for 12-inch Si wafers. A magnetic levitation stage controls the position of the wafer held by an electrostatic chuck, and an IR camera reads the alignment marks on the back of the wafer, taking advantage of the fact that Si wafers transmit infrared light. Because a mask with openings a few µm wide produces shadow if there is even a small gap to the wafer, the position and tilt are corrected before contact, and the position is then fine-tuned by moving laterally a few µm while in light contact.

Alignment precision (3σ) was ±0.0347 µm in the non-contact state and ±0.0368 µm in the final state with the mask attracted by magnets, below the target of ±0.1 µm (Figure 4). A dedicated mask transfer system exchanges masks by robot from the back of the deposition chamber, reducing the risk that organic material accumulated on the mask contaminates the wafer. Canon Tokki cited manufacturing technology for high-precision masks with openings of a few µm and mass-production cost as challenges. At Display Week 2026 it demonstrated 3,200 ppi with an electroformed Fe-Ni FMM, and it is reportedly developing a 5,000 ppi mask.

Figure 4. Canon Tokki alignment structure and alignment evaluation results

Source: Canon Tokki, presentation at the 43rd Organic EL Symposium

Sunic System has the largest supply record for 12-inch W-OLED OLEDoS evaporation equipment and holds about 85% of the OLEDoS evaporation equipment market. According to the company’s presentation, a 12-inch RGB OLEDoS evaporator requires alignment precision of 0.15 µm or better, vibration control, and a high level of thermal management, and the company stated that it can meet these requirements (Table 3). Chinese OLEDoS makers such as SeeYA (视涯科技) mass-produce W-OLED+CF panels with Sunic System equipment.

Table 3. Alignment precision of OLED evaporation equipment

EquipmentAlignment precisionSource
Mass-production OLED evaporator (G6H glass)±3 µmCanon Tokki
Micro OLED W-OLED evaporator±10–100 µmCanon Tokki
Sunic System 12" W-OLED OLEDoS evaporator< 2 µmSunic System
Sunic System Glass VR evaporator< 1 µmSunic System
Sunic System 12" RGB OLEDoS evaporator (required)< 0.15 µmSunic System
Canon Tokki 12" Si wafer RGB prototype (3σ, magnet)±0.0368 µmCanon Tokki

Source: Canon Tokki (43rd Organic EL Symposium), Sunic System (2024 Global Materials, Parts and Equipment Tech Fair); compiled by UBI Research

4. Photolithographic Patterning: SEL and Ruixian

SEL’s MML (Metal Mask-Less) process deposits the EL film over the entire surface, adds a sacrificial layer, and patterns it by lithography and dry etching, repeating this for each color. The basic process patent is US 12,262,623 B2 (granted March 25, 2025), and SEL used this method to demonstrate a 1.5-inch 3,207 ppi tandem microdisplay at 15,000 nits. On November 3, 2026, two more US patents covering device structures made by MML were granted (Table 4). Visionox (维信诺) signed a patent license with SEL in July 2025, and its own photolithography process, ViP, is for glass substrates.

China’s Ruixian Technology (睿显科技) published CN118102798A in May 2024, which patterns R, G, and B on a silicon substrate by photomask lithography. It uses a peelable organic protection layer to block moisture during wet development, and the specification states that it is an alternative to FMM.

Table 4. Photolithography-based patterning patents

CompanyItemDateKey content
SELUS 12,787,587 B22026.11.03 (granted)Separated EL layers; insulating layer contacts EL side faces under common electrode
SELUS 12,787,543 B22026.11.03 (granted)Gap between emitting units overlaps gap between pixel electrodes
SELUS 12,262,623 B22025.03.25 (granted)Base MML method with sacrificial layer
RuixianCN118102798A2024.05 (published)Photomask RGB patterning on silicon with peelable release layer

Source: USPTO Official Gazette, CNIPA.

Noh Chang-ho, chnoh@ubiresearch.com